Secondary ledeburite formation during various welding techniques
The occurrence and formation sequence of secondary ledeburite in the heat affected zone of chromium ledeburitic tool steel W.Nr. 1.2379 (OCR12 VM) after welding with SAW, TIG, microplasma and laser welding techniques is presented in this paper. Special attention was paid on the behaviour of...