Research the causes of formation of internal pores (blowholes) in welded joints of metal wire cord
Analysis of the research results shows that about 20% of defective weld joints of the metal wire cord are destroyed due to the presence of internal pores in the weld zone. The article analyzes the results of the work carried out in the laboratories of the Belarusian metallurgical works – the managem...
Saved in:
Main Authors: | I. V. Borisovets, T. P. Kurenkova, A. A. Sakharnaja |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2019-01-01
|
Series: | Литьë и металлургия |
Subjects: | |
Online Access: | https://lim.bntu.by/jour/article/view/2445 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
A study on the causes of the inconsistencies of the microstructure of welded joints of steel wire cord
by: I. V. Borisovets, et al.
Published: (2019-08-01) -
Defects of welded joints of the wire, causing breakages during drawing
by: E. S. Seregina, et al.
Published: (2018-10-01) -
Microstructure and mechanical properties of A7N01 aluminum alloy weld joints filled with ER5356 and ER5087 weld wires
by: Xie H., et al.
Published: (2022-01-01) -
Improving the Metal Inert Gas Welding Efficiency and Microstructural Stability in the Butt and Lap Joints of Aluminum Automotive Components Using Sc- and Zr-Enhanced Filler Wires
by: Hansol Ko, et al.
Published: (2024-12-01) -
Secondary ledeburite formation during various welding techniques
by: Tonkovič M.P., et al.
Published: (2015-01-01)