Effect of layer thickness ratio on microstructure and mechanical properties of TiC–WC/TiC–TiN laminated ceramics

The TiC–WC/TiC–TiN laminated ceramics with the layer thickness ratios as 2:1, 1:1, 1:2, 1:3 and 1:4, respectively, were prepared by dry pressing and vacuum hot pressing sintering with TiC as the base materials and WC and TiN as the additive phases of the TiC–WC (TW) layer and TiC–TiN (TT) layer, res...

Full description

Saved in:
Bibliographic Details
Main Authors: ZHENG Xifan, JIANG Longkai, GAO Jiaojiao, SONG Jinpeng, MENG Weiqi, WANG Yao
Format: Article
Language:zho
Published: Editorial Office of Powder Metallurgy Technology 2025-06-01
Series:Fenmo yejin jishu
Subjects:
Online Access:https://pmt.ustb.edu.cn/article/doi/10.19591/j.cnki.cn11-1974/tf.2024010012