41
-
42
The effects of initial microstructure on the creep property of a 4th generation single crystal superalloy at mediate temperature and high stress
Published 2025-03-01“…The creep properties at 800 °C and 735 MPa were examined in Ni-based single crystal superalloys (SCs) with different microstructure characteristics to systematically investigate the effects of initial microstructure on the creep property at mediate temperature and high stress. …”
Get full text
Article -
43
Thermal Mismatch Effect and High-Temperature Tensile Performance Simulation of Hybrid CMC and Superalloy Bolted Joint by Progressive Damage Analysis
Published 2020-01-01“…The hybrid CMC and superalloy bolted joints have exhibited great potential to be used as thermostructural components of reusable space transportation systems, given the respective strengths of these two materials. …”
Get full text
Article -
44
Improving oxidation resistance property of single-crystal Ni-based superalloy via utilizing high temperature aging-induced dislocations
Published 2025-03-01Subjects: “…Single crystal superalloy…”
Get full text
Article -
45
Oxidation behavior of a low-cost second-generation Ni-based single crystal superalloy at 900 °C and 1000 °C
Published 2025-01-01Subjects: “…Ni-based single crystal superalloy…”
Get full text
Article -
46
Microstructure and oxidation resistance of Pd+Zr and Pd+Hf co-doped aluminide coatings deposited on Mar-M247 nickel superalloy
Published 2023-01-01Subjects: “…nickel superalloys…”
Get full text
Article -
47
Development of TiO2-doped MgO refractories with enhanced corrosion resistance for preparing high-purity nickel-based superalloys
Published 2025-03-01Subjects: Get full text
Article -
48
-
49
Investigating the effect of optimal addition of Inconel 718 machining swarfs on the wear behavior of gray cast iron
Published 2025-03-01Subjects: Get full text
Article -
50
A novel model of the cross-section variation effect induced by contraction convection on freckle defects in directional solidification
Published 2025-03-01Subjects: “…Superalloy…”
Get full text
Article -
51
-
52
Using a Combined FE-CA Approach to Investigate Abnormally Large Grains Formed by the Limited Recrystallization Mechanism in a Powder Metallurgy Nickel-Based Superalloy
Published 2025-01-01Subjects: “…powder metallurgy nickel-based superalloy…”
Get full text
Article -
53
The effect of the amount of Y2O3 doped to the MA6000 alloy produced by mechanical alloying method on wear behavior
Published 2022-01-01Subjects: Get full text
Article -
54
-
55
Intergranular creep resistance affected by grain boundary carbides to suppress lamellae γʹ precipitation in a specially designed inconel 740H variant
Published 2025-01-01Subjects: “…Superalloys…”
Get full text
Article -
56
Tailoring graphite fiber addition to improve high-temperature wear resistance graphite fiber/ Fe composite
Published 2025-03-01Subjects: “…Ferrous superalloy…”
Get full text
Article -
57
Novel electromagnetic oscillation method for uniform grain refinement and mechanical properties enhancement of flat-shaped aerospace components
Published 2025-02-01Subjects: “…Ni-Cr-Co based superalloy…”
Get full text
Article -
58
Liquid-induced heat treatment strategy for eliminating anisotropy of IN718 fabricated by laser powder bed fusion
Published 2025-02-01Subjects: Get full text
Article -
59
Microstructure, hardness and interfacial energy in Co-9Al-10W-xNi (x=15, 25, 35 at. %) alloys during aging
Published 2017-01-01Subjects: “…Co-Al-W-Ni superalloys…”
Get full text
Article -
60
Microstructural Evolution and Oxidation Resistance of Fe-30Ni-15Cr Alloy for Internal Combustion Engine Valves Under Long-Term High-Temperature Exposure and Heat Treatment
Published 2025-01-01Subjects: “…iron–nickel-based superalloy…”
Get full text