    Characteristics of A6061/(Glass Fibre + AL2O3 + SiC + B4C) Reinforced Hybrid Composite Prepared through STIR Casting by Subramani Nanjan, Ganesh Murali Janakiram

    Published 2019-01-01
    “…Mechanical properties of the stir casting composites were evaluated through microhardness, wear test under 200 rpm and 300 rpm and 20 N and 50 N, and tensile tests. …”
    Get full text
    Article
  3. 503
  4. 504
  5. 505

    Evaluating the cost-effectiveness of prosthetic rehabilitation for partially edentulous teeth in India: A comparative study of Clasp-Retained RPDs, Thermoplastic Resin RPDs, and Cast Partial Dentures by Subhash V, Aswini Kumar K, Vineetha Karuveettil

    Published 2025-03-01
    “…Removable partial dentures (RPDs) are versatile, cost-effective solutions for partial tooth loss, including metal clasp-retained RPDs (MC-RPDs), thermoplastic resin RPDs (TR-RPDs), and cast partial dentures (CPDs). Methods: This study evaluates the oral health-related quality of life, patient satisfaction, and cost-effectiveness of these three RPD types. …”
    Get full text
    Article
  6. 506
  7. 507
  8. 508
  9. 509
  10. 510
  11. 511
  12. 512
  13. 513
  14. 514

    Effect of Heat Treatment and Titanium Addition on the Microstructure and Mechanical Properties of Cast Fe31Mn28 Ni15Al24.5Tix High-Entropy Alloys by Shimaa El-Hadad, Mervat Ibrahim, Mohamed Mourad

    Published 2019-01-01
    “…In the current investigation, Fe31Mn28 Ni15Al24.5Tix high-entropy alloys with Ti content (0–3 wt.%) were prepared by casting in an induction furnace. Different heat treatments were applied, and the microstructure and hardness of the cast samples were studied. …”
    Get full text
    Article
  15. 515

    Microstructural analysis and mechanical properties of Ni35Co25.5Al16Fe15.5Cr8 high-entropy alloy in the as-cast and homogenized conditions by A. Pourferiedouni, S.G. Shabestari

    Published 2025-01-01
    “…The true compression strength of homogenized samples exceeded 1300 MPa while the true compression strength of the as-cast sample was over 1130 MPa. The estimated ultimate strength obtained using the SP method is approximately 840 MPa for the homogenized sample, compared to 644 MPa for the as-cast sample. …”
    Get full text