Defect “steel-melting captivity and swelling” on the inner surface of seamless hot-rolled pipes. Characteristic genetic features, the causes of formation and measures of prevention...
Published 2020-01-01“…Defects found on the inner surface of the pipes are characterized as steel melting captivity and swelling. …”