Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors

Against the backdrop of limited fossil resources, bio-based plastics offer a sustainable and long-term solution. Polyamides made from bio-based raw materials (bio-PA) in particular is seen as a key driver for bio-based plastics. In the automotive industry in particular, engineering plastics such as...

Full description

Saved in:
Bibliographic Details
Main Authors: Tim Passinger, Lars Schmohl, Jan-Christoph Zarges, Julia Resch, Hans-Peter Heim, Christian Bonten
Format: Article
Language:English
Published: Elsevier 2025-05-01
Series:Polymer Testing
Subjects:
Online Access:http://www.sciencedirect.com/science/article/pii/S0142941825001102
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1850201014249979904
author Tim Passinger
Lars Schmohl
Jan-Christoph Zarges
Julia Resch
Hans-Peter Heim
Christian Bonten
author_facet Tim Passinger
Lars Schmohl
Jan-Christoph Zarges
Julia Resch
Hans-Peter Heim
Christian Bonten
author_sort Tim Passinger
collection DOAJ
description Against the backdrop of limited fossil resources, bio-based plastics offer a sustainable and long-term solution. Polyamides made from bio-based raw materials (bio-PA) in particular is seen as a key driver for bio-based plastics. In the automotive industry in particular, engineering plastics such as PA are an important product group due to their material properties. Vehicle interiors, have to meet a variety of mechanical, optical and emission-related specifications set by the manufacturer and authorities. In order to enable the use of bio-based plastics in car interiors, it is therefore necessary that they meet the manufacturers' specifications. In this context, the bio-based PA510, PA610 and PA1010 were compared with those of the fossil-based PA6 after carrying out the UV-aging process standardized in DIN75220. In order to increase the resistance of the bio-based polyamides to UV-radiation, stabilization on a twin-screw extruder was carried out and the effect was characterized after another aging cycle. The results of FTIR spectroscopy and mechanical analysis indicate that UV aging has a strong effect on the bio-based PA, as an increase in absorption has occurred at certain wave numbers (1735 and 3080) and the tensile strength and elongation at break are significantly reduced. The use of a UV-stabilizer showed the potential to mitigate these effects to a considerable extent. In addition, the emission behavior of highly volatile substances according to VDA278 was determined using GC-MS and low-volatile substances according to DIN75201. The perceived odor impression was characterized with human testers in accordance with VDA270. The tests show very low emission values in the area of VOC and SVOC for all polyamides tested. All types are suitable for use in the passenger compartment. However, the determination of the perceived odor does not meet the limit value specifications for some types.
format Article
id doaj-art-e4e75ea5154d468f85dc7f1f6676c3a4
institution OA Journals
issn 1873-2348
language English
publishDate 2025-05-01
publisher Elsevier
record_format Article
series Polymer Testing
spelling doaj-art-e4e75ea5154d468f85dc7f1f6676c3a42025-08-20T02:12:08ZengElsevierPolymer Testing1873-23482025-05-0114610879610.1016/j.polymertesting.2025.108796Investigation of the UV-aging behavior of bio-based polyamides for automotive interiorsTim Passinger0Lars Schmohl1Jan-Christoph Zarges2Julia Resch3Hans-Peter Heim4Christian Bonten5Institute of Material Engineering, Plastics Engineering, University of Kassel, Moenchebergstraße. 3, 34125, Kassel, Germany; Corresponding author.Institut für Kunststofftechnik, University of Stuttgart, Pfaffenwaldring 32, 70569, Stuttgart, GermanyInstitute of Material Engineering, Plastics Engineering, University of Kassel, Moenchebergstraße. 3, 34125, Kassel, GermanyInstitut für Kunststofftechnik, University of Stuttgart, Pfaffenwaldring 32, 70569, Stuttgart, GermanyInstitute of Material Engineering, Plastics Engineering, University of Kassel, Moenchebergstraße. 3, 34125, Kassel, GermanyInstitut für Kunststofftechnik, University of Stuttgart, Pfaffenwaldring 32, 70569, Stuttgart, GermanyAgainst the backdrop of limited fossil resources, bio-based plastics offer a sustainable and long-term solution. Polyamides made from bio-based raw materials (bio-PA) in particular is seen as a key driver for bio-based plastics. In the automotive industry in particular, engineering plastics such as PA are an important product group due to their material properties. Vehicle interiors, have to meet a variety of mechanical, optical and emission-related specifications set by the manufacturer and authorities. In order to enable the use of bio-based plastics in car interiors, it is therefore necessary that they meet the manufacturers' specifications. In this context, the bio-based PA510, PA610 and PA1010 were compared with those of the fossil-based PA6 after carrying out the UV-aging process standardized in DIN75220. In order to increase the resistance of the bio-based polyamides to UV-radiation, stabilization on a twin-screw extruder was carried out and the effect was characterized after another aging cycle. The results of FTIR spectroscopy and mechanical analysis indicate that UV aging has a strong effect on the bio-based PA, as an increase in absorption has occurred at certain wave numbers (1735 and 3080) and the tensile strength and elongation at break are significantly reduced. The use of a UV-stabilizer showed the potential to mitigate these effects to a considerable extent. In addition, the emission behavior of highly volatile substances according to VDA278 was determined using GC-MS and low-volatile substances according to DIN75201. The perceived odor impression was characterized with human testers in accordance with VDA270. The tests show very low emission values in the area of VOC and SVOC for all polyamides tested. All types are suitable for use in the passenger compartment. However, the determination of the perceived odor does not meet the limit value specifications for some types.http://www.sciencedirect.com/science/article/pii/S0142941825001102Bio-PAUV-AgingAutomotive interiorOdorGC-MSVOC
spellingShingle Tim Passinger
Lars Schmohl
Jan-Christoph Zarges
Julia Resch
Hans-Peter Heim
Christian Bonten
Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
Polymer Testing
Bio-PA
UV-Aging
Automotive interior
Odor
GC-MS
VOC
title Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
title_full Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
title_fullStr Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
title_full_unstemmed Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
title_short Investigation of the UV-aging behavior of bio-based polyamides for automotive interiors
title_sort investigation of the uv aging behavior of bio based polyamides for automotive interiors
topic Bio-PA
UV-Aging
Automotive interior
Odor
GC-MS
VOC
url http://www.sciencedirect.com/science/article/pii/S0142941825001102
work_keys_str_mv AT timpassinger investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors
AT larsschmohl investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors
AT janchristophzarges investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors
AT juliaresch investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors
AT hanspeterheim investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors
AT christianbonten investigationoftheuvagingbehaviorofbiobasedpolyamidesforautomotiveinteriors