Influence of deoxidizing powder on the internal surface of hot-rolled pipes
The article describes the experience of using deoxidizing powder in the technological process of production of hot-rolled seamless pipes; the processes that occur when applying to the inner surface of the hollow billet deoxidizing powder. The results of experimental and industrial tests of deoxidizi...
Saved in:
Main Author: | O. V. Rozhkova |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2019-04-01
|
Series: | Литьë и металлургия |
Subjects: | |
Online Access: | https://lim.bntu.by/jour/article/view/2707 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Algorithm for optimization of cold‑rolled pipe rolling routes
by: S. V. Pilipenko
Published: (2024-09-01) -
CHANGING THE PROPERTIES OF THE STEEL 10G2BF AFTER HOT ROLLING
by: A. B. Steblov, et al.
Published: (2016-08-01) -
Defect “steel-melting captivity and swelling” on the inner surface of seamless hot-rolled pipes. Characteristic genetic features, the causes of formation and measures of prevention.
by: I. A. Kovaleva, et al.
Published: (2020-01-01) -
Piping systems : Drafting and Design /
by: Lamit Louis Gary
Published: (1981) -
Studies and Research on the Replacement of Pipes Made of Steel P355N, Intended for Domestic Water
by: Beatrice Daniela TUDOR, et al.
Published: (2024-09-01)