Microstructure and Hardness of Cold Work Vanadis 6 Steel after Subzero Treatment at −140°C
The microstructure, phase constitution, and hardness of Cr-V ledeburitic tool steel Vanadis 6 subjected to subzero treatment at −140°C and for different soaking times have been investigated. The light microscopy, scanning electron microscopy, and X-ray diffraction have been used for microstructural...