Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel
Temperature intervals of oxide reduction processes during sintering of the Fe-3%Cr-0.5%Mo prealloyed powder using continuous monitoring of processing-exhaust gas composition (CO, CO2, and H2O) were identified and interpreted in relation to density (6.5–7.4 g/cm3), sintering temperature (1120 and 120...