The Shear Bond Strength of Porcelain Bonding to Cobalt-Chromium Dental Alloys Before and After Thermal Cycling
Metal-ceramic crowns and bridges provide a stable and aesthetic tooth reconstruction. Hot pressing of veneering ceramics to metal substructure minimizes the formation of pores. Within the oral cavity, prosthetic structures are exposed to thermal stress. The study examines the influence of temperatur...
Saved in:
Main Authors: | Ewa Pruszczyńska, Zofia Kula, Katarzyna Dąbrowska, Leszek Klimek |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2024-12-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/15/1/12 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Bond Strength of Porcelain Fused to Casting and Selective Laser Base Metal Alloy with a Bonding Agent
by: Rafal Kareem Rasheed, et al.
Published: (2022-09-01) -
Comparison of Debonding of Different Composite Resin Bonds and Acrylic Tooth with Acrylic Denture Base after Thermocycling Regimes.
by: Aso M. Zangana, et al.
Published: (2024-06-01) -
Air Particle Abrasion in Dentistry: An Overview of Effects on Dentin Adhesion and Bond Strength
by: Andreea Kui, et al.
Published: (2024-12-01) -
Classification of RTV-coated porcelain insulator condition under different profiles and levels of pollution
by: Ali Ahmed Salem, et al.
Published: (2024-10-01) -
Minimally invasive rehabilitation with porcelain veneers: case report
by: Danela Cisneros Boada, et al.
Published: (2019-01-01)