Formation and growth mechanism of the α2 lath within the γ phase in high Nb containing TiAl alloy
A high Nb containing TiAl alloy exhibiting near fully lamellar microstructure with nano-lamellar spacing was obtained via heat treatment. The lamellar structure exhibits an average spacing of approximately 75 nm and comprises both γ/α₂ and γ/γ interfaces. Subsequent multiaxial compression led to the...
Saved in:
Main Authors: | Gengwu Ge, Gang Yang, Yingchao Guo, Yongfeng Liang, Junpin Lin |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2025-03-01
|
Series: | Journal of Materials Research and Technology |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2238785425001310 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Evolution mechanisms of the scratch-induced elastoplastic stress fields and crack damage in γ-TiAl alloys
by: Zhaoqing Zhang, et al.
Published: (2025-01-01) -
Parametric programming of CNC lathes
by: Vasilić Goran V., et al.
Published: (2024-01-01) -
Effects of Machining Parameters on Abrasive Flow Machining of Single Crystal γ-TiAl Alloy Based on Molecular Dynamics
by: Junye Li, et al.
Published: (2025-01-01) -
Effects of plasma surface Ta alloying on the tribology behavior of γ-TiAl
by: Wei D.-B., et al.
Published: (2021-01-01) -
Microstructural investigation of the coatings prepared by simultaneous aluminizing and siliconizing process on γ-TiAl
by: Nouri S., et al.
Published: (2019-01-01)