Analysis of Degradation Mechanisms in LiNi0.8Mn0.1Co0.1O2 Lithium-ion Battery Cathodes During High-Rate Charge–Discharge Cycling
The increasing demand for cobalt reduction and high energy density in lithium-ion batteries has accelerated the development of cathode-active materials based on Ni-rich layered oxides. However, Ni-rich cathodes, such as LiNi0.8Mn0.1Co0.1O2 (NMC811), suffer from capacity degradation due to factors in...
Saved in:
| Main Authors: | Daisuke SHIBATA, Rinka YAMAMOTO, Mao MATSUMOTO, Haruno MURAYAMA, Chengchao ZHONG, Keiji SHIMODA, Ken-ichi OKAZAKI, Shohei YAMASHITA, Yuki ORIKASA |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
The Electrochemical Society of Japan
2025-06-01
|
| Series: | Electrochemistry |
| Subjects: | |
| Online Access: | https://www.jstage.jst.go.jp/article/electrochemistry/93/6/93_25-71043/_html/-char/en |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Synthesis of nano cubic microstructure LiNi0.8Co0.1Mn0.1O2 cathode materials via rapid precipitation assisted with hydrothermal treatment
by: Jing Lao, et al.
Published: (2024-11-01) -
Norbornenic anhydride as versatile additive optimizing interphases to enable high-performance LiNi0.8Co0.1Mn0.1O2/Li batteries
by: Fujie Yang, et al.
Published: (2025-04-01) -
An overview on the structure and electrochemical properties of Co-free Ni-rich LiNi0.8Mn0.1Fe0.1O2 as a cathode material for lithium-ion batteries
by: Rasha S. El-Tawil, et al.
Published: (2025-08-01) -
Sintesis Material Katoda LiNi0,8Mn0,1Co0,1O2 (NMC811) dengan Metode Solid State Menggunakan Nikel Hasil Perolehan Kembali dari Spent Nickel Catalyst
by: Hendri Widiyandari, et al.
Published: (2022-09-01) -
Exploring electrochemical dynamics in graphite||LiNi0.8Mn0.1Co0.1O2 cells via operando ultrasound and multiprobe approaches
by: Corentin Renais, et al.
Published: (2025-08-01)