Antimony recovery from recycled terminals of lead-acid batteries with Na2CO3 and SiC after firstly SsB2O3 formation
Terminals obtained from spent lead-acid batteries in Mexico contain around 2 wt% Sb. The terminals were melted in an electric furnace and then oxygen was injected at 750 °C with a gas flow rate of 2 L/min to produce high purity Sb2O3. The antimony trioxide obtained was treated with a mixture of Na2C...
Saved in:
Main Authors: | Jiménez-Lugos J.C., Sánchez-Alvarado R.G., Cruz-Ramírez A., Romero-Serrano J.A., Hernández-Ramírez A., Rivera-Salinas J.E. |
---|---|
Format: | Article |
Language: | English |
Published: |
University of Belgrade, Technical Faculty, Bor
2022-01-01
|
Series: | Journal of Mining and Metallurgy. Section B: Metallurgy |
Subjects: | |
Online Access: | http://www.doiserbia.nb.rs/img/doi/1450-5339/2022/1450-53392100052J.pdf |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
High antimony resistance strain Enterobacter sp. Z1 mediates biomineralization of antimony trioxide
by: Zijie Zhou, et al.
Published: (2025-01-01) -
Removal of lead from crude antimony by using NaPo3 as lead elimination reagent
by: Ye L.G., et al.
Published: (2015-01-01) -
Kinetics of stibnite (Sb2S3) oxidation at roasting temperatures
by: Padilla R., et al.
Published: (2014-01-01) -
Non-diaphragm electrodeposition of antimony: Effect of process parameters and precipitating agents
by: Morcali M.H., et al.
Published: (2022-01-01) -
Antimony production by carbothermic reduction of stibnite in the presence of lime
by: Padilla R., et al.
Published: (2014-01-01)