DETERMINATION OF POSSIBLE REASONS OF FORMATION OF DEFECT «MICROPITTING» IN HARD-ALLOY DIE INSTRUMENT IN THE PROCESS OF WIRE DRAWING
It is established that during operating time in the working channel of die along with uniform scuffing the stable wear occurs as a result of welding of metal particles to die material, what leads to formation of separate micropockets.
Saved in:
Main Authors: | T. P. Kurenkova, I. P. Lazebnikova, T. N. Lipatkina |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2011-09-01
|
Series: | Литьë и металлургия |
Online Access: | https://lim.bntu.by/jour/article/view/670 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
DETERMINATION OF POSSIBLE REASONS OF DEFECT FORMATION «MICROPITTING» IN HARD-ALLOY WIRE DRAWING INSTRUMENT IN WIRE DRAWING PROCESS
by: T. P. Kurenkova, et al.
Published: (2011-05-01) -
ANALYSIS OF POSSIBLE REASONS OF FOMIATION OF NODULAR CEMENTITE IN STRUCTURE OF WIRE OF HIGH-CARBON STEEL IN CONDITIONS OF HARDWARE PRODUCTION OF RUP “BMZ”
by: T. P. Kurenkova, et al.
Published: (2008-08-01) -
Defects of welded joints of the wire, causing breakages during drawing
by: E. S. Seregina, et al.
Published: (2018-10-01) -
WIRE BREAKAGE DURING WIRE DRAWING DUE TO THE PRESENCE OF SURFACE DEFECTS, INHERITED FROM WIRE ROD
by: A. S. Siarohina
Published: (2018-01-01) -
THE INFLUENCE OF MORPHOLOGY OF DIAMOND SYNTHETIC MICROPOWDER ON QUALITY OF PROCESSING OF THE CHANNEL OF CARBIDE DRAWING DIES
by: E. S. Eltsova, et al.
Published: (2017-10-01)