Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading

Purpose. Porcelain laminate veneers (PLVs) are sometimes required to be used for teeth with composite fillings. This study examined the fracture strength of PLVs bonded to the teeth restored with different sizes of class V composite fillings. Materials and Methods. Thirty-six maxillary central incis...

Full description

Saved in:
Bibliographic Details
Main Authors: Leyla Sadighpour, Farideh Geramipanah, Vanya Rasaei, Mohammad J. Kharazi Fard
Format: Article
Language:English
Published: Wiley 2018-01-01
Series:International Journal of Dentistry
Online Access:http://dx.doi.org/10.1155/2018/1456745
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1832565085114990592
author Leyla Sadighpour
Farideh Geramipanah
Vanya Rasaei
Mohammad J. Kharazi Fard
author_facet Leyla Sadighpour
Farideh Geramipanah
Vanya Rasaei
Mohammad J. Kharazi Fard
author_sort Leyla Sadighpour
collection DOAJ
description Purpose. Porcelain laminate veneers (PLVs) are sometimes required to be used for teeth with composite fillings. This study examined the fracture strength of PLVs bonded to the teeth restored with different sizes of class V composite fillings. Materials and Methods. Thirty-six maxillary central incisors were divided into three groups (n=12): intact teeth (control) and teeth with class V composite fillings of one-third or two-thirds of the crown height (small or large group, resp.). PLVs were made by using IPS e.max and bonded with a resin cement (RelyX Unicem). Fracture resistance (N) was measured after cyclic loading (1 × 106 cycles, 1.2 Hz). For statistical analyses, one-way ANOVA and Tukey test were used (α=0.05). Results. There was a significant difference between the mean failure loads of the test groups (P=0.004), with the Tukey-HSD test showing lower failure loads in the large-composite group compared to the control (P=0.02) or small group (P=0.05). The control and small-composite groups achieved comparable results (P>0.05). Conclusions. Failure loads of PLVs bonded to intact teeth and to teeth with small class V composite fillings were not significantly different. However, extensive composite fillings could compromise the bonding of PLVs.
format Article
id doaj-art-2f3aa62c1c2a4dcc80ae859b07557b28
institution Kabale University
issn 1687-8728
1687-8736
language English
publishDate 2018-01-01
publisher Wiley
record_format Article
series International Journal of Dentistry
spelling doaj-art-2f3aa62c1c2a4dcc80ae859b07557b282025-02-03T01:09:30ZengWileyInternational Journal of Dentistry1687-87281687-87362018-01-01201810.1155/2018/14567451456745Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic LoadingLeyla Sadighpour0Farideh Geramipanah1Vanya Rasaei2Mohammad J. Kharazi Fard3Department of Prosthodontics, Faculty of Dentistry, Tehran University of Medical Sciences, Tehran, IranDental Implant Research Center, Faculty of Dentistry, Tehran University of Medical Sciences, Tehran, IranDepartment of Prosthodontics, Faculty of Dentistry, Tehran University of Medical Sciences, Tehran, IranDental Research Center, Faculty of Dentistry, Tehran University of Medical Sciences, Tehran, IranPurpose. Porcelain laminate veneers (PLVs) are sometimes required to be used for teeth with composite fillings. This study examined the fracture strength of PLVs bonded to the teeth restored with different sizes of class V composite fillings. Materials and Methods. Thirty-six maxillary central incisors were divided into three groups (n=12): intact teeth (control) and teeth with class V composite fillings of one-third or two-thirds of the crown height (small or large group, resp.). PLVs were made by using IPS e.max and bonded with a resin cement (RelyX Unicem). Fracture resistance (N) was measured after cyclic loading (1 × 106 cycles, 1.2 Hz). For statistical analyses, one-way ANOVA and Tukey test were used (α=0.05). Results. There was a significant difference between the mean failure loads of the test groups (P=0.004), with the Tukey-HSD test showing lower failure loads in the large-composite group compared to the control (P=0.02) or small group (P=0.05). The control and small-composite groups achieved comparable results (P>0.05). Conclusions. Failure loads of PLVs bonded to intact teeth and to teeth with small class V composite fillings were not significantly different. However, extensive composite fillings could compromise the bonding of PLVs.http://dx.doi.org/10.1155/2018/1456745
spellingShingle Leyla Sadighpour
Farideh Geramipanah
Vanya Rasaei
Mohammad J. Kharazi Fard
Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
International Journal of Dentistry
title Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
title_full Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
title_fullStr Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
title_full_unstemmed Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
title_short Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading
title_sort fracture resistance of ceramic laminate veneers bonded to teeth with class v composite fillings after cyclic loading
url http://dx.doi.org/10.1155/2018/1456745
work_keys_str_mv AT leylasadighpour fractureresistanceofceramiclaminateveneersbondedtoteethwithclassvcompositefillingsaftercyclicloading
AT faridehgeramipanah fractureresistanceofceramiclaminateveneersbondedtoteethwithclassvcompositefillingsaftercyclicloading
AT vanyarasaei fractureresistanceofceramiclaminateveneersbondedtoteethwithclassvcompositefillingsaftercyclicloading
AT mohammadjkharazifard fractureresistanceofceramiclaminateveneersbondedtoteethwithclassvcompositefillingsaftercyclicloading