HARDENING OF CASTINGS AT FREE FORMING OF INTERNAL SURFACE
The reasons of arising of the hollow castings polythickness at free forming of internal surface are investigated. The recommendations on its reduction are given
Saved in:
Main Authors: | E. I. Marukovich, V. F. Bevza, V. P. Grusha |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2005-08-01
|
Series: | Литьë и металлургия |
Online Access: | https://lim.bntu.by/jour/article/view/1882 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
LONGITUDINAL DIFFERENT-WALL OF HOLLOW CASTINGS AT FORMING OF INTERNAL SURFACE OUT OF MELT WITHOUT APPLICATION OF ROD
by: E. I. Marukovich, et al.
Published: (2006-05-01) -
CONTINUOUSLY AND CYCLIC CASTING BY SILVERING OF PIPE SLUGS
by: E. I. Marukovich, et al.
Published: (2014-03-01) -
REFINEMENT OF CASTINGS AT CASTING BY DIRECTIONAL HARDENING
by: E. I. Marukovich, et al.
Published: (2005-05-01) -
THEORETICAL AND TECHNOLOGICAL BASIS OF CASTING OF HOLLOW BILLETS BY THE METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2011-05-01) -
INCREASING OF STEADINESS OF THE CRYSTALLIZER COOLING AT CASTING OF DIRECTIONAL HARDENING
by: E. I. Marukovich, et al.
Published: (2005-05-01)