Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials

Concrete, widely used in construction, presents sustainability issues due to its significant environmental footprint. An eco-friendly substitute, alkali-activated concrete (AAC), significantly lowers carbon di-oxide (CO2) emissions and energy requirements. In comparison to conventional Portland ceme...

Full description

Saved in:
Bibliographic Details
Main Authors: R. Samuvel Raj, G. Prince Arulraj, N. Anand, Balamurali Kanagaraj, Eva Lubloy, Paul Joseph
Format: Article
Language:English
Published: Elsevier 2025-07-01
Series:Case Studies in Construction Materials
Subjects:
Online Access:http://www.sciencedirect.com/science/article/pii/S2214509525001287
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1832087466409984000
author R. Samuvel Raj
G. Prince Arulraj
N. Anand
Balamurali Kanagaraj
Eva Lubloy
Paul Joseph
author_facet R. Samuvel Raj
G. Prince Arulraj
N. Anand
Balamurali Kanagaraj
Eva Lubloy
Paul Joseph
author_sort R. Samuvel Raj
collection DOAJ
description Concrete, widely used in construction, presents sustainability issues due to its significant environmental footprint. An eco-friendly substitute, alkali-activated concrete (AAC), significantly lowers carbon di-oxide (CO2) emissions and energy requirements. In comparison to conventional Portland cement (OPC), AAC demonstrates superior fire resistance, ensuring structural integrity in elevated temperature environments. The inclusion of additives further enhances AAC's durability and thermal properties. This research explores the impact of nano- fly ash (nFA), nano-ground granulated blast furnace slag (nGS), and nano-bentonite (nBT) on the properties of alkali-activated nano concrete (AANC) when subjected to high temperatures. While there is substantial research on conventional concrete, AANC, especially its high-temperature performance, remains under-explored. This study addresses this gap by examining how these nanomaterials (NM) affect the workability, mechanical properties, and thermal stability of AANC. The study shows that increasing the content of nFA, nGS, and nBT leads to a reduction in slump values, signifying decreased workability. Optimal levels of nFA and nGS significantly improve the mechanical strength due to enhanced particle packing and microstructural compactness. However, excessive amounts of these NM result in strength reduction due to particle agglomeration. nBT exhibits a complex relationship with compressive strength (CS), with an optimal dosage beyond which strength decreases. Elevated-temperature tests showed that nGS12 specimens had the highest CS at ambient temperature. Residual compressive strength (RCS) increased up to 400 °C but sharply declined at 600 °C and 800 °C. nGS specimens demonstrated superior thermal performance, while nBT specimens experienced significant strength loss. Flexural strength (FS) and splitting tensile strength (STS) significantly decreased with increasing temperature, with nBT-blended AANC showing the largest crack widths. Microstructural analysis through X-ray diffraction (XRD) and scanning electron microscopy (SEM) indicated substantial changes at elevated temperatures, such as increased porosity and gel phase decomposition. Thermogravimetric analysis (TGA) analysis indicated reduced weight loss (WL) in nanomaterial-enhanced AANC, suggesting better thermal stability. These findings highlight the need to optimize nanomaterial content to achieve a balance between mechanical performance and thermal stability in AANC.
format Article
id doaj-art-2648ec096f1240a39b37db261303071d
institution Kabale University
issn 2214-5095
language English
publishDate 2025-07-01
publisher Elsevier
record_format Article
series Case Studies in Construction Materials
spelling doaj-art-2648ec096f1240a39b37db261303071d2025-02-06T05:11:48ZengElsevierCase Studies in Construction Materials2214-50952025-07-0122e04330Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterialsR. Samuvel Raj0G. Prince Arulraj1N. Anand2Balamurali Kanagaraj3Eva Lubloy4Paul Joseph5Department of Civil Engineering, Karunya Institute of Technology and Sciences, Coimbatore, IndiaDepartment of Civil Engineering, Karunya Institute of Technology and Sciences, Coimbatore, IndiaDepartment of Civil Engineering, Karunya Institute of Technology and Sciences, Coimbatore, India; Corresponding authors.Department of Civil Engineering, Karunya Institute of Technology and Sciences, Coimbatore, IndiaDepartment of Construction Materials and Technologies, Budapest University of Technology and Economics, Budapest 1521, Hungary; Corresponding authors.Institute of Sustainable and Liveable Cities, Victoria University, Melbourne, AustraliaConcrete, widely used in construction, presents sustainability issues due to its significant environmental footprint. An eco-friendly substitute, alkali-activated concrete (AAC), significantly lowers carbon di-oxide (CO2) emissions and energy requirements. In comparison to conventional Portland cement (OPC), AAC demonstrates superior fire resistance, ensuring structural integrity in elevated temperature environments. The inclusion of additives further enhances AAC's durability and thermal properties. This research explores the impact of nano- fly ash (nFA), nano-ground granulated blast furnace slag (nGS), and nano-bentonite (nBT) on the properties of alkali-activated nano concrete (AANC) when subjected to high temperatures. While there is substantial research on conventional concrete, AANC, especially its high-temperature performance, remains under-explored. This study addresses this gap by examining how these nanomaterials (NM) affect the workability, mechanical properties, and thermal stability of AANC. The study shows that increasing the content of nFA, nGS, and nBT leads to a reduction in slump values, signifying decreased workability. Optimal levels of nFA and nGS significantly improve the mechanical strength due to enhanced particle packing and microstructural compactness. However, excessive amounts of these NM result in strength reduction due to particle agglomeration. nBT exhibits a complex relationship with compressive strength (CS), with an optimal dosage beyond which strength decreases. Elevated-temperature tests showed that nGS12 specimens had the highest CS at ambient temperature. Residual compressive strength (RCS) increased up to 400 °C but sharply declined at 600 °C and 800 °C. nGS specimens demonstrated superior thermal performance, while nBT specimens experienced significant strength loss. Flexural strength (FS) and splitting tensile strength (STS) significantly decreased with increasing temperature, with nBT-blended AANC showing the largest crack widths. Microstructural analysis through X-ray diffraction (XRD) and scanning electron microscopy (SEM) indicated substantial changes at elevated temperatures, such as increased porosity and gel phase decomposition. Thermogravimetric analysis (TGA) analysis indicated reduced weight loss (WL) in nanomaterial-enhanced AANC, suggesting better thermal stability. These findings highlight the need to optimize nanomaterial content to achieve a balance between mechanical performance and thermal stability in AANC.http://www.sciencedirect.com/science/article/pii/S2214509525001287Alkali-activated concretenanomaterialsnano-fly ashnano-GGBFSnano-bentoniteresidual properties
spellingShingle R. Samuvel Raj
G. Prince Arulraj
N. Anand
Balamurali Kanagaraj
Eva Lubloy
Paul Joseph
Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
Case Studies in Construction Materials
Alkali-activated concrete
nanomaterials
nano-fly ash
nano-GGBFS
nano-bentonite
residual properties
title Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
title_full Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
title_fullStr Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
title_full_unstemmed Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
title_short Elevated-temperature performance of alkali-activated nano concrete: The role of sustainable nanomaterials
title_sort elevated temperature performance of alkali activated nano concrete the role of sustainable nanomaterials
topic Alkali-activated concrete
nanomaterials
nano-fly ash
nano-GGBFS
nano-bentonite
residual properties
url http://www.sciencedirect.com/science/article/pii/S2214509525001287
work_keys_str_mv AT rsamuvelraj elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials
AT gprincearulraj elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials
AT nanand elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials
AT balamuralikanagaraj elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials
AT evalubloy elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials
AT pauljoseph elevatedtemperatureperformanceofalkaliactivatednanoconcretetheroleofsustainablenanomaterials