The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins

The insufficiently binder between acrylic teeth and dentures is considered to be the primary cause of teeth fractures from the dentures and is one of the disadvantages of acrylic denture base material. This research has been conducted to assess various concentrations of Nano hydroxyapatite addition...

Full description

Saved in:
Bibliographic Details
Main Author: Hawraa khalid Aziz
Format: Article
Language:English
Published: middle technical university 2023-09-01
Series:Journal of Techniques
Subjects:
Online Access:https://journal.mtu.edu.iq/index.php/MTU/article/view/982
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1832595169763917824
author Hawraa khalid Aziz
author_facet Hawraa khalid Aziz
author_sort Hawraa khalid Aziz
collection DOAJ
description The insufficiently binder between acrylic teeth and dentures is considered to be the primary cause of teeth fractures from the dentures and is one of the disadvantages of acrylic denture base material. This research has been conducted to assess various concentrations of Nano hydroxyapatite addition on the shear bond between repaired acrylic teeth and polymer. One-hundred specimens of resin were split into two main subdivisions. 50 specimens were repaired with cold cured Duracryl Plus and the other 50 were repaired with a special type of acrylic O-cry1. Each one was sectioned into tested groups depending on (1%., 2%., 3%, and 5% by wt. of nano hydroxyapatite) incorporation and control group (0% of nano hydroxyapatite) with (n=10). The Universal testing machine was utilized for shear bond strength measurement. The obtained values were diffracted by t-test, ANOVA, and LSD-test. There was an increase in bond strength that repairing with O-cry1 than Duracryl Plus with a heightening in the bond strength, which was seen with incorporating nano hydroxyapatite into the acrylic resin with a significant difference between them. The 2% wt. Nano hydroxyapatite group demonstrated the maximum mean values, while those for the 5% wt. Nano hydroxyapatite group were recording minimum value with a significant difference between them. Repairing with O-cry1 recording better bond strength than Duracryl Plus acrylic. Furthermore, the addition of hydroxyapatite in Nano-form has successfully improved the “shear bond strength” of teeth to the PMMA at 2% wt. nano hydroxyapatite.
format Article
id doaj-art-1ebb0aee77674081b2b7ea4305989efc
institution Kabale University
issn 1818-653X
2708-8383
language English
publishDate 2023-09-01
publisher middle technical university
record_format Article
series Journal of Techniques
spelling doaj-art-1ebb0aee77674081b2b7ea4305989efc2025-01-19T10:55:26Zengmiddle technical universityJournal of Techniques1818-653X2708-83832023-09-015310.51173/jt.v5i3.982The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic ResinsHawraa khalid Aziz0College of Health & Medical Technology - Baghdad, Middle Technical University, Baghdad, Iraq The insufficiently binder between acrylic teeth and dentures is considered to be the primary cause of teeth fractures from the dentures and is one of the disadvantages of acrylic denture base material. This research has been conducted to assess various concentrations of Nano hydroxyapatite addition on the shear bond between repaired acrylic teeth and polymer. One-hundred specimens of resin were split into two main subdivisions. 50 specimens were repaired with cold cured Duracryl Plus and the other 50 were repaired with a special type of acrylic O-cry1. Each one was sectioned into tested groups depending on (1%., 2%., 3%, and 5% by wt. of nano hydroxyapatite) incorporation and control group (0% of nano hydroxyapatite) with (n=10). The Universal testing machine was utilized for shear bond strength measurement. The obtained values were diffracted by t-test, ANOVA, and LSD-test. There was an increase in bond strength that repairing with O-cry1 than Duracryl Plus with a heightening in the bond strength, which was seen with incorporating nano hydroxyapatite into the acrylic resin with a significant difference between them. The 2% wt. Nano hydroxyapatite group demonstrated the maximum mean values, while those for the 5% wt. Nano hydroxyapatite group were recording minimum value with a significant difference between them. Repairing with O-cry1 recording better bond strength than Duracryl Plus acrylic. Furthermore, the addition of hydroxyapatite in Nano-form has successfully improved the “shear bond strength” of teeth to the PMMA at 2% wt. nano hydroxyapatite. https://journal.mtu.edu.iq/index.php/MTU/article/view/982Hydroxyapatite NanoparticlesAcrylic TeethHeat Cure AcrylicShear Bond StrengthO-cry1
spellingShingle Hawraa khalid Aziz
The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
Journal of Techniques
Hydroxyapatite Nanoparticles
Acrylic Teeth
Heat Cure Acrylic
Shear Bond Strength
O-cry1
title The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
title_full The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
title_fullStr The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
title_full_unstemmed The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
title_short The Effect of Nano Hydroxyapatite on the Bond Strength of Acrylic Teeth Repaired to an Acrylic Resin Denture Base Using Two Types of Auto Polymerized Acrylic Resins
title_sort effect of nano hydroxyapatite on the bond strength of acrylic teeth repaired to an acrylic resin denture base using two types of auto polymerized acrylic resins
topic Hydroxyapatite Nanoparticles
Acrylic Teeth
Heat Cure Acrylic
Shear Bond Strength
O-cry1
url https://journal.mtu.edu.iq/index.php/MTU/article/view/982
work_keys_str_mv AT hawraakhalidaziz theeffectofnanohydroxyapatiteonthebondstrengthofacrylicteethrepairedtoanacrylicresindenturebaseusingtwotypesofautopolymerizedacrylicresins
AT hawraakhalidaziz effectofnanohydroxyapatiteonthebondstrengthofacrylicteethrepairedtoanacrylicresindenturebaseusingtwotypesofautopolymerizedacrylicresins