DC Electrical Ageing of XLPE under Hydrostatic Pressure
The experimental electrical ageing, of cross-linked polyethylene films 100 μm thick, was investigated under high hydrostatic pressure of 300 bar and at atmospheric pressure. The tests are conducted on direct current (dc) for up to 1000 h ageing and at temperature of 70°C. The use of the Weibull stat...
Saved in:
Main Authors: | Fadila Benlizidia Lalam, Faouzi Djemmal |
---|---|
Format: | Article |
Language: | English |
Published: |
Wiley
2017-01-01
|
Series: | Advances in Materials Science and Engineering |
Online Access: | http://dx.doi.org/10.1155/2017/3936163 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Simulation and validation of the effect of hydrostatic and non-hydrostatic pressure on contact pressure in a resilient seat butterfly valve
by: K Yuvaraj, et al.
Published: (2025-01-01) -
Rigorous Solution of Slopes’ Stability considering Hydrostatic Pressure
by: Chengchao Li, et al.
Published: (2018-01-01) -
Effects of Hydrostatic Pocket Shape on the Flow
Pattern and Pressure Distribution
by: M. J. Braun, et al.
Published: (1995-01-01) -
Partial discharges characteristics study in XLPE cable insulation with multiple defects
by: I. V. Komarov, et al.
Published: (2021-12-01) -
Study power of partial discharges to voltage intensity in XLPE-insulated cables
by: D. A. Polyakov, et al.
Published: (2020-03-01)